From: Sustainable solidification of ferrochrome slag through geopolymerisation: a look at the effect of curing time, type of activator and liquid solid ratio
Sample
Fe (ppm)
Zn (ppm)
Mn (ppm)
Ni (ppm)
Cr (ppm)
GP0
45.7
1.23
1.78
3.76
15.7
GPS1
7.45
1.33
1.44
7.54
GPA2
1.34
1.24
0.88
1.21