From: Sustainable solidification of ferrochrome slag through geopolymerisation: a look at the effect of curing time, type of activator and liquid solid ratio
Sample
Fe (mg m− 2)
Zn (mg m− 2)
Mn (mg m− 2)
Ni (mg m− 2)
Cr (mg m− 2)
GP0
3043
82
119
251
1044
GPS1
497
89
96
503
GPA2
83
59
81