Skip to main content

Table 1 BET surface area (SBET) and pore volume (Vpore) of the as-synthesized samples

From: Chitosan@TiO2 composites for the adsorption of copper(II) and antibacterial applications

Samples

SBET (m2 g− 1)a

Vpore (cm3 g− 1)b

3%CS-V

30

0.026

3%CST-V

10

0.011

5%CS-V

28

0.019

5%CST-V

5

0.006

7%CS-V

29

0.034

7%CST-V

9

0.028

3%CS-X

2

0.010

3%CST-X

40

0.12

5%CS-X

24

0.017

5%CST-X

22

0.071

7%CS-X

21

0.035

7%CST-X

18

0.049

  1. a BET specific surface area; b Total pore volume measured at P/P0 = 0.99