Fig. 7From: Combination of rGO/S, N/TiO2 for the enhancement of visible light-driven toluene photocatalytic degradationPhotocatalytic degradation of toluene under various (a, b) initial concentration, (c, d) relative humidity/RH, (e, f) temperature, and (g, h) retention timeBack to article page